Abstract

Since geothermal wells are a feasible energy source to replace fossil fuel supply, many technologies have been developed to take advantage of geothermal energy. Nevertheless, service conditions in geothermal facilities are due to the chemical composition of hydrothermal fluids and temperatures, in many cases, extreme in terms of corrosion. Therefore, materials selection based on preliminary material qualification is essential to guarantee a secure and reliable operation of the facilities.
The corrosion behavior of different high-alloyed metals including duplex and austenitic stainless steels as well as a nickel alloy have been evaluated in artificial geothermal fluids simulating the conditions in some locations with geothermal potential in Germany as well as two sites in Indonesia.
The suitability of carbon steel 25CrMo4, stainless steels X2CrNiMo17-12-2, X2CrNiMo-22-5, X2CrNiMoCuWN25-7-4 and super austenitic steel X1CrNiMoCu32-28-7 in these geothermal fluids obtained by electrochemical measurements and exposure tests is limited. The nickel alloy NiCr23Mo16Al shows an excellent corrosion resistance against pitting corrosion. Excluding its high cost, it is a very good alternative to be used in the construction of geothermal facilities having highly saline brines. Stainless and duplex steels exhibit a limited corrosion resistance concerning pitting and crevice corrosion.
Beside of the higher alloyed materials, also the low-alloyed steel 25CrMo4 could be employed as a constructional material for the geothermal power plant in stagnant highly acidic non saline environments, as long as the wall thickness of the material vs. corrosion rate is taken into account.

Copyright 2016, EGEC / EGC2016. Readers who download papers from this site should honour the copyright of the original authors, and may not copy or distribute the work further without the permission of the original publisher.